Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 13.7 W/m-K | 95.1 BTU-in/hr-ft²-°F | |
California Fine Wire Stablohm 710 Nickel Chromium Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Thermal Conductivity | 13.7 W/m-K @Temperature 20.0 - 100 °C |
95.1 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367) The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Thermal Conductivity | 13.7 W/m-K @Temperature 20.0 - 100 °C |
95.1 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 10% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Thermal Conductivity | 13.7 W/m-K @Temperature 20.0 - 100 °C |
95.1 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 20% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Thermal Conductivity | 13.7 W/m-K @Temperature 20.0 - 100 °C |
95.1 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 30% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Thermal Conductivity | 13.7 W/m-K @Temperature 20.0 - 100 °C |
95.1 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 40% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Thermal Conductivity | 13.7 W/m-K @Temperature 20.0 - 100 °C |
95.1 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 50% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Thermal Conductivity | 13.7 W/m-K @Temperature 20.0 - 100 °C |
95.1 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 60% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Thermal Conductivity | 13.7 W/m-K @Temperature 20.0 - 100 °C |
95.1 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 75% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |