Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.30 W/m-K | 9.02 BTU-in/hr-ft²-°F | |
Permabond ES578 Epoxy Resin PERMABOND® ES578 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces, ceramics as well as composite materials. ES578 provides excellent thermal conductivity and bon.. |
|||
Thermal Conductivity | 1.30 W/m-K | 9.02 BTU-in/hr-ft²-°F | in-plane, ø80*3mm discs; ISO 22007-2 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6 Eco-FR compound |
|||
Thermal Conductivity | 1.30 W/m-K | 9.02 BTU-in/hr-ft²-°F | in-plane, ø80*3mm discs; ISO 22007-2 |
SABIC Innovative Plastics LNP KONDUIT PX11311U PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6 compliant with ECO protocols, non-brominated, non chlorinated |
|||
Thermal Conductivity | 1.30 W/m-K | 9.02 BTU-in/hr-ft²-°F | In-Plane; ASTM E-1461 |
Victrex® APTIV® 1103-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, Mineral Filled
(Unve Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a.. |
|||
Thermal Conductivity | 1.30 W/m-K | 9.02 BTU-in/hr-ft²-°F | In-Plane; ASTM E1461 |
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a.. |
|||
Thermal Conductivity | 1.30 W/m-K | 9.02 BTU-in/hr-ft²-°F | Average; ISO/CD 22007-4 |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
Thermal Conductivity | 1.30 W/m-K | 9.02 BTU-in/hr-ft²-°F | Average; ISO/CD 22007-4 |
Victrex® WG102™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c.. |
|||
Thermal Conductivity | 1.30 W/m-K | 9.02 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® T7109-19 Electrically Insulating Epoxy Paste Material Description: A flexible, thermally conductive, electrically insulating epoxy paste designed for low stress and heat dissipation applications. It is an alternative to EPO-TEK® T7109-17, de.. |