Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 116 W/m-K | 805 BTU-in/hr-ft²-°F | |
California Fine Wire Nickel Alloy 30 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |