Thermal Properties Metric English Comments
Thermal Conductivity 11.2 W/m-K
77.7 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® B-3® alloy, 0% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 11.2 W/m-K
77.7 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® B-3® alloy, 10% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 11.2 W/m-K
77.7 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® B-3® alloy, 20% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 11.2 W/m-K
77.7 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 11.2 W/m-K
77.7 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® B-3® alloy, 30% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 11.2 W/m-K
77.7 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® B-3® alloy, 40% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 11.2 W/m-K
77.7 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® B-3® alloy, 50% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 11.2 W/m-K
77.7 BTU-in/hr-ft²-°F
Special Metals INCONEL® Alloy 601
A nickel-chromium alloy with an addition of aluminum for outstanding resistance to oxidation and other forms of high-temperature corrosion. It also has high mechanical properties at elevated temper..
Thermal Conductivity 11.2 W/m-K
77.7 BTU-in/hr-ft²-°F
Special Metals NIMONIC® Alloy 80A
A nickel-chromium alloy similar to NIMONIC alloy 75 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good corrosion and oxidation resistance and high tensile a..
Thermal Conductivity 11.2 W/m-K

@Temperature 0.000 - 100 °C
77.7 BTU-in/hr-ft²-°F

@Temperature 32.0 - 212 °F
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Sheet and Strip, UNS N07718
Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro..
Thermal Conductivity 11.2 W/m-K

@Temperature 0.000 - 100 °C
77.7 BTU-in/hr-ft²-°F

@Temperature 32.0 - 212 °F
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Plate, UNS N07718
Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro..
Thermal Conductivity 11.2 W/m-K
77.7 BTU-in/hr-ft²-°F
RT
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea..
Thermal Conductivity 11.2 W/m-K

@Temperature 0.000 - 100 °C
77.7 BTU-in/hr-ft²-°F

@Temperature 32.0 - 212 °F
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated plus Precipitation Heat Treated, UNS N07718
Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro..