Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 100 - 130 W/m-K | 694 - 902 BTU-in/hr-ft²-°F | |
MarkeTech AN 120 Aluminum Nitride Ceramic Substrate, 98% Purity Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µ.. |
|||
Thermal Conductivity | 100 W/m-K | 694 BTU-in/hr-ft²-°F | |
MMCC Al/Al2O3 Short Fiber Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Thermal Conductivity | 100 W/m-K | 694 BTU-in/hr-ft²-°F | |
Sapco S.SiC Silicon Carbide Information provided by Sapco. |
|||
Thermal Conductivity | 100 W/m-K | 694 BTU-in/hr-ft²-°F | |
UCAR Carbon UCAR® ATR Isostatic Molded Graphite Isostatically molded ATR is a lower density version of grade ATJ. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish.Typical Application.. |
|||
Thermal Conductivity | 100 W/m-K @Temperature 20.0 - 100 °C |
694 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
DIN EN 821-2 |
CeramTec CD 101 Silicon Carbide, SiC-ZrB2 CD101 is a zirconia reinforced silicon carbide designed for maximum hardness. |
|||
Thermal Conductivity | 100 W/m-K | 694 BTU-in/hr-ft²-°F | DIN EN 821-2 |
CeramTec CD 110 Silicon Carbide, SSiC Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. It outstanding sliding properties and high thermal conductivity make useful in tribological applicati.. |
|||
Thermal Conductivity | 100 W/m-K | 694 BTU-in/hr-ft²-°F | DIN EN 821-2 |
CeramTec Rocar® ST Silicon Carbide, SSiC Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. Its outstanding sliding properties and high thermal conductivity make useful in tribological applicat.. |
|||
Thermal Conductivity | 100 W/m-K | 694 BTU-in/hr-ft²-°F | |
CoorsTek ACI-Co6 Tungsten Carbide Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries |
|||
Thermal Conductivity | 100 W/m-K | 694 BTU-in/hr-ft²-°F | ASTM C408 |
CoorsTek SC-BNL (SC-42) Loaded Reaction Bonded Silicon Carbide Thermal Shock Delta Tc = 137°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Thermal Conductivity | 100 W/m-K | 694 BTU-in/hr-ft²-°F | ASTM C408 |
CoorsTek Tungsten Carbide, WC Information provided by CoorsTek. |