Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 9.10 W/m-K | 63.2 BTU-in/hr-ft²-°F | |
Kennametal Stellite Stellite® 250 Resistant to heat, thermal shock, thermal cycling, oxidation, and hot corrosion from flue gas, slags, and molten copper. Not recommended for use in abrasive wear.Applications:heat treatment furnace.. |
|||
Thermal Conductivity | 9.10 W/m-K | 63.2 BTU-in/hr-ft²-°F | RT |
Haynes Hastelloy® C-2000® alloy, flat products Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 9.10 W/m-K | 63.2 BTU-in/hr-ft²-°F | |
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening.. |