Polymer Property : Thermal Conductivity = 60.0 BTU-in/hr-ft²-°F
Polymer Property :
Thermal Conductivity =
60.0 BTU-in/hr-ft²-°F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Thermal Conductivity
8.65
W/m-K
60.0
BTU-in/hr-ft²-°F
Cotronics Resbond™ 931 High Temperature Graphite Adhesive