Polymer Property : Thermal Conductivity = 6.09 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.878 W/m-K
6.09 BTU-in/hr-ft²-°F
Atom Adhesives AA-BOND F162 Epoxy Adhesive
AA-BOND F162 is a thixotropic electrical insulating epoxy adhesive system with low vapor pressure and outgassing characteristics. AA-BOND F162 was specifically developed for fiber optic, laser, phot..