Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 86.0 W/m-K @Temperature 85.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® 4 Pure Indium Solder Soft, ductile metal has good wettability on many surfaces including ceramics, glass and quartz. Deforms indefinitely under load and has no tendency to become brittle, making it valuable for cryogeni.. |
|||
Thermal Conductivity | 86.0 W/m-K | 597 BTU-in/hr-ft²-°F | |
Special Metals Nickel 270 A high-purity grade of nickel made by powder metallurgy. It has a low base hardness and high ductility. Its extreme purity is useful for components of hydrogen thyratrons. It is also used for ele.. |
|||
Thermal Conductivity | 86.0 W/m-K | 597 BTU-in/hr-ft²-°F | |
Tokuyama Shapal™ SH-50 Sintered Aluminum Nitride Uniform, large sized pressed sintered aluminum nitride. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899A 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899A 1/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899A 3/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899A Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899A Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899D 50% Cold-Rolled Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899D Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899E 50% Cold-Rolled Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899E Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899L 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899L 1/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899L 3/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899L Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899L Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899L Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899L Skin Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899M 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899M 1/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899M Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899M Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899M Skin Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899A Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899A Skin Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899G 50% Cold-Rolled Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899G Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899M 3/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Thermal Conductivity | 86.0 W/m-K @Temperature 70.0 °C |
597 BTU-in/hr-ft²-°F @Temperature 158 °F |
|
Ametek High Purity Nickel Strip 899M Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |