Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 75.0 W/m-K | 521 BTU-in/hr-ft²-°F | |
Hogen HM1100 Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers hig.. |
|||
Thermal Conductivity | 75.0 W/m-K | 521 BTU-in/hr-ft²-°F | |
MMCC Al/B4C Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Thermal Conductivity | 75.0 W/m-K | 521 BTU-in/hr-ft²-°F | |
Mi-Tech Metals HD17D Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; ASTM B-777-07 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Slightly Magnetic.Manufactured by powder metallurgy methods. The t.. |
|||
Thermal Conductivity | >= 75.0 W/m-K | >= 521 BTU-in/hr-ft²-°F | |
H.C. Starck HPM 1750 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Thermal Conductivity | >= 75.0 W/m-K | >= 521 BTU-in/hr-ft²-°F | |
H.C. Starck HPM 1760 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Thermal Conductivity | >= 75.0 W/m-K | >= 521 BTU-in/hr-ft²-°F | |
H.C. Starck HPM 1750 Tungsten High Density Composite Sheet Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for further processing by the custo.. |
|||
Thermal Conductivity | >= 75.0 W/m-K | >= 521 BTU-in/hr-ft²-°F | |
H.C. Starck HPM 1850 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Thermal Conductivity | 75.0 W/m-K | 521 BTU-in/hr-ft²-°F | |
Special Metals Nickel 205 Wrought nickel similar to Nickel 200 but with compositional adjustments to enhance performance in electrical and electronic applications. Ferromagnetic. Used for the anodes and grids of electronic.. |
|||
Thermal Conductivity | 75.0 W/m-K | 521 BTU-in/hr-ft²-°F | |
CoorsTek ACI-Ni10 Tungsten Carbide Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries |
|||
Thermal Conductivity | 75.0 W/m-K | 521 BTU-in/hr-ft²-°F | |
CMW® ELKALOY D110 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |