Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.810 W/m-K @Temperature 80.0 °C |
5.62 BTU-in/hr-ft²-°F @Temperature 176 °F |
ASTM C518 |
Rogers Corporation RO3210 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Thermal Conductivity | 0.810 W/m-K | 5.62 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only.. |
|||
Thermal Conductivity | 0.810 W/m-K | 5.62 BTU-in/hr-ft²-°F | |
Schott N-KZFS11 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.810 W/m-K | 5.62 BTU-in/hr-ft²-°F | |
Schott N-LASF40 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.810 W/m-K | 5.62 BTU-in/hr-ft²-°F | |
Schott N-LASF43 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.810 W/m-K | 5.62 BTU-in/hr-ft²-°F | |
Schott N-SSK2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.810 W/m-K | 5.62 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI) Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not .. |
|||
Thermal Conductivity | 0.810 W/m-K | 5.62 BTU-in/hr-ft²-°F | |
Schott N-KZFS2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.810 W/m-K | 5.62 BTU-in/hr-ft²-°F | |
Schott N-LAK33A Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.810 W/m-K | 5.62 BTU-in/hr-ft²-°F | ASTM C-518 |
Sumitomo Bakelite North America SI 9002N-1 Silicone Compound Short fibergass reinforced silicone molding compound which offers moderate strength properties, dimensional stability, and excellent long-term thermal stability at elevated temperatures.Information .. |
|||
Thermal Conductivity | 0.810 W/m-K | 5.62 BTU-in/hr-ft²-°F | |
Loctite® 3151 1 component acrylic UV/Heat Cure Acrylic Adhesive Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |
|||
Thermal Conductivity | 0.810 W/m-K @Temperature 121 °C |
5.62 BTU-in/hr-ft²-°F @Temperature 250 °F |
|
Tra-Con Tra-Bond 161-3 Temperature Resistant Epoxy Adhesive TRA-BOND 161-3 two component, premixed and frozen, epoxy adhesive is highly filled. This electrically insulating adhesive provides structural strength to 150°C and semi structural strength to 300°.. |
|||
Thermal Conductivity | 0.810 W/m-K | 5.62 BTU-in/hr-ft²-°F | ASTM E1461 |
Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards Only Woven Glass Reinforced PTFE/Ceramic with Dk of 10.2 or greaterHigh Copper Peel Strength allows for thinner etched line widthsLowest insertion loss availableLarger Panel sizes availableLow moist.. |