Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 71.0 W/m-K | 493 BTU-in/hr-ft²-°F | |
CMW® ELKALOY D120 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |