Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 590 W/m-K | 4090 BTU-in/hr-ft²-°F | |
Cytec Thornel® P-100 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus fibers consisting of 2000 filaments in a one-ply construction.0.32 m/g yield, 0 or 32 tpm t.. |