Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 59.0 W/m-K | 409 BTU-in/hr-ft²-°F | Parallel to pressing direction |
Momentive Performance Materials HBN Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Thermal Conductivity | 59.0 W/m-K | 409 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS199 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 59.0 W/m-K | 409 BTU-in/hr-ft²-°F | |
California Fine Wire Nickel 220 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Thermal Conductivity | 59.0 W/m-K | 409 BTU-in/hr-ft²-°F | |
California Fine Wire Nickel 271 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Thermal Conductivity | 59.0 W/m-K | 409 BTU-in/hr-ft²-°F | |
California Fine Wire Nickel 272 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Thermal Conductivity | 59.0 W/m-K | 409 BTU-in/hr-ft²-°F | |
California Fine Wire Nickel 5900 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Thermal Conductivity | 59.0 W/m-K | 409 BTU-in/hr-ft²-°F | |
California Fine Wire Nickel Alloy 99 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |