Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | ASTM D5470 |
Parker Chomerics PREMIER™ A240-FRHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | ASTM D5470 |
Parker Chomerics PREMIER™ A240-HTHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Cookson Group Plaskon® 3400 Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A reduced-stress epoxy molding compound for the encapsulation of a variety of semiconductor devices ranging from small lead count.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Cookson Group Plaskon® 3400FP Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A fast curing, reduced-stress epoxy molding compound for the encapsulation of semiconductor devices including DIPs, PLCCs, SOICs .. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Cookson Group Plaskon® S-7LA Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices. It offers an alpha par.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Cookson Group Plaskon® S-7P Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low viscosity epoxy encapsulant designed for packaging stress-sensitive semiconductor devices. It is specifically .. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® BMC 0160 Unsaturated Polyester UP BMC 0160 is a general purpose BMC for electrical applications. Typical applications are lamp housings, canopies, covers and similar components.Information Provided by Menzolit |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® BMC 0400 Unsaturated Polyester UP BMC 0400 is a low profile DMC/BMC for automotive applications. It fulfills the requirements of the automotive industry regarding painted body panels including reduced C-emissions. For highest surfac.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® MMC 1600 Unsaturated Polyester UP MMC 1600 is a mineral moulding compound (similar to DMC/BMC) providing of a stone like appearance eg. granite or marble. Chrome plated mould surfaces are required. It is recommended that product thi.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP SMC 0390 is a standard low profile SMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surfac.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 0430 Unsaturated Polyester UP SMC 0430 is a low emission Class-A SMC for on-line painted exterior body applications on passenger cars. These compounds mould to parts with excellent surface quality for on-line painted body panel.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 0520 Unsaturated Polyester UP SMC 0520 is a special SMC with significantly reduced density. The glass level has been selected to combine good moulding with sufficient strength and stiffness properties. Even without a specific fi.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 1000 Unsaturated Polyester UP SMC 1000 is a special SMC for hydrolysis resistant applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Typical applications are .. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 1650 Unsaturated Polyester UP SMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® BMC 0300 Unsaturated Polyester UP BMC 0300 is a low shrink standard material for general-purpose applications, which require a higher level on surface quality and better dimensional stability. The glass content is on a level that co.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® BMC 2300 Unsaturated Polyester UP BMC 2300 is a special BMC with exceptional high fire retardancy. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Fire retardanc.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® BMC 2600 Unsaturated Polyester UP BMC 2600 is a special BMC with reduced electrical properties. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. Because of its improved.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® BMC 3000 Unsaturated Polyester UP BMC 3000 is a special BMC suitable for the use in microwave and cookware applications.It has high temperature resistance, and meets requirements for food contact applications. It has a high gloss fi.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® BMC 3100 Unsaturated Polyester UP BMC 3100 is a special BMC suitable for the use in head lamp reflectors. Because of its high temperature resistance and dimensional stability as well as low coefficient of thermal expansion, complex .. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets .. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 0290 Unsaturated Polyester UP SMC 0290 is a specially formulated SMC processable by injection moulding. The gentle production process prevents the fiber from any damage. Parts made of SMC 0290 reach higher levels of strength and.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
Menzolit Menzolit® SMC 2500 Unsaturated Polyester UP SMC 2500 is a special SMC for high voltage isolating applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Even without a specific.. |
|||
Thermal Conductivity | 0.700 W/m-K @Temperature 90.0 °C |
4.86 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8531 Soft Glass Soft glass, free from Na, of high lead content, high dielectric constant Encapsulation of semiconductor components at low temperature (diodes)Information provided by SCHOTT AG. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK) AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th.. |
|||
Thermal Conductivity | 0.700 W/m-K @Temperature 100 °C |
4.86 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 1501 Polyester, Briquette, Compression Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | ASTM E1225 |
3D Systems DuraForm® PA Nylon for SLS® Systems For use with all selective laser sintering (SLS®) systems.ApplicationsComplex, thin-wall ductworkMotorsportsAerospaceHousings and enclosuresImpellers and connectorsConsumer sporting goodsVehicle da.. |
|||
Thermal Conductivity | 0.700 W/m-K @Temperature 200 °C |
4.86 BTU-in/hr-ft²-°F @Temperature 392 °F |
DIN 52612 |
Brandenburger ISOFLEX AFV Foam This material is a noncombustible, inorganic, flexible insulating foam used as exterior lining to save thermal energy, mainly in the rubber and plastics industry. It is also used in the refrigeratio.. |