Thermal Properties Metric English Comments
Thermal Conductivity 0.511 W/m-K
3.55 BTU-in/hr-ft²-°F
Sharadaa Ceramics REFINSUL 15LI Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Thermal Conductivity <= 0.511 W/m-K

@Temperature 500 °C
<= 3.55 BTU-in/hr-ft²-°F

@Temperature 932 °F
Sharadaa Ceramics REFINSUL ZAP-020 Insulating Castables
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l..