Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 344 W/m-K | 2390 BTU-in/hr-ft²-°F | |
OMG Americas GlidCop® AL-25 Dispersion Strengthened Copper GlidCop® AL-25 is copper that is dispersion strengthened with 0.5 wt% ultrafine particles of aluminum oxide. It is produced using an internal oxidation powder metallurgy process whereby aluminum o.. |
|||
Thermal Conductivity | 345 W/m-K | 2390 BTU-in/hr-ft²-°F | |
CMW® DSC Copper with Dispersed Aluminum Oxide CMW® DSC material is an extruded and cold worked powder metallurgy material consisting of copper and dispersed aluminum oxide. It has exceptional high temperature strength for its electrical conduc.. |