Thermal Conductivity 34.5 W/m-K

@Temperature 95.0 °C
239 BTU-in/hr-ft²-°F

@Temperature 203 °F
Crucible Steel HALGRAPH® Tool Steel, AISI O6
Halgraph is an oil-hardening graphitic tool steel with excellent non-deforming properties. Free graphite in its structure affords exceptional free-machining properties. The combination of graphite a..
Thermal Conductivity 34.5 W/m-K

@Temperature 95.0 °C
239 BTU-in/hr-ft²-°F

@Temperature 203 °F
Crucible Steel KETOS® Tool Steel, AISI O1
Ketos is an oil-hardening tool steel which may be hardened from fairly low temperatures with little size change. This grade combines deep-hardening qualities with a fine-grained structure, affording..