Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 32.9 W/m-K @Temperature 1200 °C |
228 BTU-in/hr-ft²-°F @Temperature 2190 °F |
|
Haynes HR-160® alloy plate, aged 1000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 32.9 W/m-K @Temperature 1200 °C |
228 BTU-in/hr-ft²-°F @Temperature 2190 °F |
|
Haynes HR-160® alloy plate, aged 4000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 32.9 W/m-K @Temperature 1200 °C |
228 BTU-in/hr-ft²-°F @Temperature 2190 °F |
|
Haynes HR-160® alloy, annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 32.9 W/m-K @Temperature 1200 °C |
228 BTU-in/hr-ft²-°F @Temperature 2190 °F |
|
Haynes HR-160® alloy, plate, aged 1000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 32.9 W/m-K @Temperature 1200 °C |
228 BTU-in/hr-ft²-°F @Temperature 2190 °F |
|
Haynes HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 32.9 W/m-K @Temperature 1200 °C |
228 BTU-in/hr-ft²-°F @Temperature 2190 °F |
|
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 32.9 W/m-K @Temperature 1200 °C |
228 BTU-in/hr-ft²-°F @Temperature 2190 °F |
|
Haynes HR-160® alloy, plate, aged 4000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 32.9 W/m-K @Temperature 1200 °C |
228 BTU-in/hr-ft²-°F @Temperature 2190 °F |
|
Haynes HR-160® alloy, plate, aged 8000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 32.9 W/m-K @Temperature 1200 °C |
228 BTU-in/hr-ft²-°F @Temperature 2190 °F |
|
Haynes HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 32.9 W/m-K @Temperature 1200 °C |
228 BTU-in/hr-ft²-°F @Temperature 2190 °F |
|
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 32.9 W/m-K | 228 BTU-in/hr-ft²-°F | |
SGL Carbon Group EK 305 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Thermal Conductivity | 32.9 W/m-K | 228 BTU-in/hr-ft²-°F | |
Eagle Brass 752 Nickel Silver 18%, 1/2 Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Thermal Conductivity | 32.9 W/m-K | 228 BTU-in/hr-ft²-°F | |
Eagle Brass 752 Nickel Silver 18%, 1/4 Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Thermal Conductivity | 32.9 W/m-K | 228 BTU-in/hr-ft²-°F | |
Eagle Brass 752 Nickel Silver 18%, 3/4 Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Thermal Conductivity | 32.9 W/m-K | 228 BTU-in/hr-ft²-°F | |
Eagle Brass 752 Nickel Silver 18%, Annealed Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Thermal Conductivity | 32.9 W/m-K | 228 BTU-in/hr-ft²-°F | |
Eagle Brass 752 Nickel Silver 18%, Extra Spring Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Thermal Conductivity | 32.9 W/m-K | 228 BTU-in/hr-ft²-°F | |
Eagle Brass 752 Nickel Silver 18%, Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Thermal Conductivity | 32.9 W/m-K | 228 BTU-in/hr-ft²-°F | |
Eagle Brass 752 Nickel Silver 18%, Spring Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Thermal Conductivity | 32.9 W/m-K | 228 BTU-in/hr-ft²-°F | |
Eagle Brass 752 Nickel Silver 18%, Extra Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |