Polymer Property : Thermal Conductivity = 2250 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 324 W/m-K
2250 BTU-in/hr-ft²-°F
CMW® 3 Copper Alloy
CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre..