Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 32.31 W/m-K | 224.2 BTU-in/hr-ft²-°F | |
Dura-Bar 100-70-03 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Thermal Conductivity | 32.31 W/m-K | 224.2 BTU-in/hr-ft²-°F | |
Dura-Bar 120-90-02 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |