Thermal Properties Metric English Comments
Thermal Conductivity 31.1 W/m-K

@Temperature 1100 °C
216 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes HR-160® alloy plate, aged 1000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 31.1 W/m-K

@Temperature 1100 °C
216 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes HR-160® alloy plate, aged 4000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 31.1 W/m-K

@Temperature 1100 °C
216 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes HR-160® alloy, annealed plate
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 31.1 W/m-K

@Temperature 1100 °C
216 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes HR-160® alloy, plate, aged 1000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 31.1 W/m-K

@Temperature 1100 °C
216 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 31.1 W/m-K

@Temperature 1100 °C
216 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 31.1 W/m-K

@Temperature 1100 °C
216 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes HR-160® alloy, plate, aged 4000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 31.1 W/m-K

@Temperature 1100 °C
216 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes HR-160® alloy, plate, aged 8000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 31.1 W/m-K

@Temperature 1100 °C
216 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 31.1 W/m-K

@Temperature 1100 °C
216 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 31.1 W/m-K
216 BTU-in/hr-ft²-°F
Chicago Extruded Metals BioBrass® CXM10 Lead-Free Alloy
Finished product available in rods.Chicago Extruded Metal temper code: H02This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Copyright © lookpolymers.com All Rights Reserved