Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | |
Orbilan ORBILAN® PE 1000 UHMW-PE Orbilan PE 1000 plastics distinguish themselves through their optimal balance of the technical features with regard to wear-resistance and impact resistance. The areas of use range from general mac.. |
|||
Thermal Conductivity | 0.410 W/m-K @Temperature 700 °C |
2.85 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Pyrotek Pyrocast HD Castable Refractory Pyrocast HD is an insulating castable which is particularly suitable in applications where a combination of low thermal conductivity and long service life is required.ApplicationsLaunder lining Hot-.. |
|||
Thermal Conductivity | 0.410 - 0.790 W/m-K | 2.85 - 5.48 BTU-in/hr-ft²-°F | Average value: 0.583 W/m-K Grade Count:3 |
Overview of materials for Phenolic, Resole, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | |
Mikro-Technik Mikrolen UHMW-PE Properties: very good impact resistance / high absorption at shock and impact stress extremely high resistance against abrasive wear good corrosion resistance highly resistant at temperatures of -26.. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | ASTM D C177 |
Isoflon PTFE + 25% Glass Polytetrafluoroethylene with 25% Glass Properties:Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityApplications: Dynamic seals with rotating or alternating motion.Information provided by Iso.. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | |
Momentive Performance Materials TSE3940 Flame Retardant Adhesive Sealant, Gray TSE3940 and TSE3941 flame retardant adhesive/sealants are non-flowable, one-component RTVs that cure quickly by reacting with atmospheric moisture forming a soft elastic silicone rubber. These mater.. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | ASTM C518 |
Sumitomo Bakelite North America RX® 613 Fiberglass Reinforced Phenolic RX 613 is a fiberglass reinforced phenolic molding compound with good dimensional stability and good strength at elevated temperatures.Information provided by Sumitomo Bak North America, Inc. |
|||
Thermal Conductivity | 0.410 W/m-K @Temperature 100 °C |
2.85 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 2311 Phenolic, Granular, Compression Molded PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr.. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | Moulding Direction; ASTM C177 |
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures.. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | Moulding Direction; ASTM C177 |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | ASTM E1461 |
Vyncolit A2990 Glass Fiber Reinforced Novolac Phenolic Resole resin based, glass fiber reinforced. Good mechanical properties, combined with superior electrical insulation properties. Among others used for commutator applicationsInformation provided by .. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | across thickness of mat |
Cytec Thornel® Mat VMA Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Composed of high strength, high modulus carbon filaments in a random-layered orientation. The fine diameter filaments are up to th.. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | across thickness of mat |
Cytec Thornel® Mat VMC Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Prepared by sectioning mat VMA into cubes ~ 0.5x0.5x1.0 in. VMC can be heterogeneously dispersed in matrix materials and thus enha.. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | across thickness of mat |
Cytec Thornel® Mat VMD Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Form of mat VMA with shorter fibers for injection molding. Fiber lengths average 400 µm - adequate for good property improvement... |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | across thickness of mat |
Cytec Thornel® Mat VME Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Form of mat VMA with shorter fibers for injection molding. Fiber lengths average 200 µm - inadequate for good mechanical property.. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | Moulding Direction; ASTM C177 |
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures.. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | Moulding Direction; ASTM C177 |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | |
Hippe PE 1000 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | |
Hippe PE 500 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Algoflon® 25GL PTFE; Glass Fiber Filled
(discontinued **) Data provided by the manufacturer.25 wt.% Glass Fiber. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almos.. |
|||
Thermal Conductivity | 0.410 W/m-K | 2.85 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROLEN PE-UHMW Ultra-high molecular weight polyethylene This plastic is a low density, easily machined material that can be welded and has a low sliding friction with high impact resistance. Applications include glide strips, pump components, and wearin.. |