Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | |
Permabond ET505 Epoxy Resin PERMABOND ET505 is a two-part, 1:1 mixable epoxy adhesive. ET505 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | |
Permabond ET510 Epoxy Resin PERMABOND ET510 is a two-part, 1:1 mixable epoxy adhesive. ET510 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM E1461 |
Park Electrochemical Nelco® N4380-13 RF Microwave Performance, Modified Epoxy The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,.. |
|||
Thermal Conductivity | 0.350 W/m-K @Temperature 23.0 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Along flow; ISO/CD 22007-4 |
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | Average value: 0.350 W/m-K Grade Count:3 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-8099 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 19/CF/30 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 46/CF/15 Polyamide 46, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Fluorseals PTFE 15% glass filled Improved compressive strength and wear resistance.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Fluorseals PTFE 25% glass filled Improved compressive strength and wear resistance.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105/GF/20/EM PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105/GF/20/EM/RD PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-8001 PEEK, with glass spheres Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM C177 |
Unitika UNILATE® 1 SC PET Antistatic gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and ot.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ISO 8302 |
Eurostar Starflam AFR682B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 401 PTFE, 10% Polyimide Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 403 PTFE, 15% Polyimide Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 436 PTFE, 15% Ekonol® Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | |
Trelleborg Emerson & Cuming Stycast® 2741-15 Two-Component Epoxy Flexible Encapsulant Emerson & Cuming 2741-15 Stycast® Two-Component Epoxy Flexible EncapsulantDescriptionElectronic embedment and sealing of metals, ceramics, and plastics. Protection of stress sensitive components wh.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | C518/C177 |
Saint-Gobain Meldin® 2030 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3WG5 BK 00654 PA6 25% Glass Filled BK (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical.. |