Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.342 W/m-K | 2.37 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Nylatron® MC® 901 Blue, Heat Stabilized, Type 6 (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic ProductsBroadest size range availabilityGood mechanical and electrical propertiesIdeal balance of strength and toughnessCast as finished parts and near .. |
|||
Thermal Conductivity | 0.342 W/m-K | 2.37 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Nylatron® WP PA (ASTM Product Data Sheet) |