Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 201 PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 201 PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 203 PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 203R PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Ensinger ENSITEP® PET Polyethylene Terephthalate - Extruded Products
(discontinued **) ENSITEP is an unreinforced, semi-crystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus, and .. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM E1530 |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 101 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated, 7.0 MFR, for thicker sections without sinks. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM E1461 |
Park Electrochemical Nelco® N4000-12 SI® High Speed/Low Loss, CAF Resistant Laminate and Prepreg The Nelco® N4000-12 series is an enhanced epoxy resin system designed for use in high speed, low loss applications requiring thermal stability, excellent signal speed and CAF resistance.Key Feature.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | DOM 52612 |
Manifattura Cattaneo PET+PTFE Polyethylene Terephthalate Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Thermal Conductivity | 0.290 - 0.380 W/m-K | 2.01 - 2.64 BTU-in/hr-ft²-°F | ASTM F433 |
Garlock 2920 Compressed Aramid Fiber Gasketing, SBR Binder Aramid fibers with a SBR binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, steam, inert gases, mild acids and mild alkaliesInform.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | DIN 52612 |
GEHR Plastics PET Polyethylene Terephthalate Polyethylene terephthalate shows high tensile and mechanical strength, hardness and toughness, low friction and a high dimensional stability. PET may be used at temperatures ranging from -20°C to.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ISO 8301:1991 |
Global EPP PET SL PET + Solid Lubricant PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV8111 White General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Haysite H254 Polyester Laminate Solder Pallet and Work Holder Sheet A Static dissipative sheet material for use in electronic assembly. Resistant to hot solder and solvents. Standard color is blue/grey. Available thicknesses from.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
Glastic Laminates/Shapes MTS Grade MTS Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon PUR Polyurethane Very high wear resistanceHighly resilientInformation provided by Isoflon. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | DIN 52612 |
Schwartz Technical Plastics LAMINEX® 2000 Cotton Fabric, Phenolic Resin Impregnated, Coarse Application: rollneck-bearings, coverts for friction rollsInformation provided by Schwartz Technical Plastics GmbH |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 2410F PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). UL94 V0 and 5VA listing. US FDA and European Food contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM PW2300 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified... |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Dow CYCLOTENE™ 3022-35 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Dow CYCLOTENE™ 3022-63 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Dow CYCLOTENE™ 4026-46 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ 4026-46 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Dow CYCLOTENE™ XU35075 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ XU35075 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ISO 8302 |
Eurostar Staramide A28N PA66, Nucleated, Injection Molding Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROMID 6 G Polyamide 6 Cast This material has good machinability and can be bonded or welded. Its applications include sliding bearings, hammerheads, and toothed gears.Information provided by CENTROPLAST Engineering Plastics .. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM E 1530 |
Arlon 51228R015 Silicone Rubber/Fiberglass Laminate Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultradur S 4090 G6 30% Glass Filled PBT Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | Estimated from similar grades. |
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |