Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 28.7 W/m-K @Temperature 1000 °C |
199 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Haynes HR-160® alloy plate, aged 1000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 28.7 W/m-K @Temperature 1000 °C |
199 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Haynes HR-160® alloy plate, aged 4000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 28.7 W/m-K @Temperature 1000 °C |
199 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Haynes HR-160® alloy, annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 28.7 W/m-K @Temperature 1000 °C |
199 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Haynes HR-160® alloy, plate, aged 1000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 28.7 W/m-K @Temperature 1000 °C |
199 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Haynes HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 28.7 W/m-K @Temperature 1000 °C |
199 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 28.7 W/m-K @Temperature 1000 °C |
199 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Haynes HR-160® alloy, plate, aged 4000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 28.7 W/m-K @Temperature 1000 °C |
199 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Haynes HR-160® alloy, plate, aged 8000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 28.7 W/m-K @Temperature 1000 °C |
199 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Haynes HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 28.7 W/m-K @Temperature 1000 °C |
199 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |