Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 24.9 W/m-K @Temperature 20.0 °C |
173 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Schmolz + Bickenbach 416 Stainless Steel Bar Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity.. |
|||
Thermal Conductivity | 24.9 W/m-K @Temperature 20.0 °C |
173 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Schmolz + Bickenbach 430FR Stainless Steel Bar Description: Ugitech’s 430FR is a ferritic stainless steel designed for soft magnetic components operating in corrosive environments. The 17.00% - 18.00% chromium makes corrosion resistance sim.. |
|||
Thermal Conductivity | 24.9 W/m-K @Temperature 93.0 °C |
173 BTU-in/hr-ft²-°F @Temperature 199 °F |
|
Crucible Steel CSM® 420 XL Stainless Steel CSM 420 XL is the workhorse premium quality stainless mold steel designed for applications requiring a combination of corrosion resistance and wear resistance. It is double melted for the microstruc.. |
|||
Thermal Conductivity | 24.9 W/m-K @Temperature 100 °C |
173 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Crucible Steel Maxel® 2000 Stainless Steel Maxel 2000 is a free-machining stainless holder block steel which is based on the nominal analysis of Type 414L rather than Type 420. It is supplied pre-hardened to about HRC 37. Due to its unique c.. |
|||
Thermal Conductivity | 24.9 W/m-K | 173 BTU-in/hr-ft²-°F | |
AK Steel 420 Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
Thermal Conductivity | 24.9 W/m-K | 173 BTU-in/hr-ft²-°F | |
AK Steel 420 ULTRA HONE® Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
Thermal Conductivity | 24.9 W/m-K | 173 BTU-in/hr-ft²-°F | |
AK Steel 420HC Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
Thermal Conductivity | 24.9 W/m-K | 173 BTU-in/hr-ft²-°F | |
AK Steel 420LC Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
Thermal Conductivity | 24.9 W/m-K @Temperature 100 °C |
173 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum 410 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Thermal Conductivity | 24.9 W/m-K | 173 BTU-in/hr-ft²-°F | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 482°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Thermal Conductivity | 24.9 W/m-K | 173 BTU-in/hr-ft²-°F | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 593°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Thermal Conductivity | 24.9 W/m-K | 173 BTU-in/hr-ft²-°F | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 649°C (1200°F) (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Thermal Conductivity | 24.9 W/m-K | 173 BTU-in/hr-ft²-°F | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 760°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Thermal Conductivity | 24.9 W/m-K | 173 BTU-in/hr-ft²-°F | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 538°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Thermal Conductivity | 24.9 W/m-K | 173 BTU-in/hr-ft²-°F | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 704°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |