Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.46 W/m-K | 10.2 BTU-in/hr-ft²-°F | |
Aremco AREMCOLOX™ 502-800 Macor Glass Ceramic
(Unverified Data**) Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and .. |