Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.272 W/m-K | 1.88 BTU-in/hr-ft²-°F | |
Cytec EN-2521 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Thermal Conductivity | 0.272 W/m-K | 1.88 BTU-in/hr-ft²-°F | |
Cytec EN-2532 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |