Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet) This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resis.. |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Nylatron® GF30 Nylon Type 66, 30% Glass-Reinforced Black Color (ASTM Product Data Sheet) |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet) |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Quadrant Nylon 101 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet) |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM C177 |
Quantum Nylon 6/6 Information provided by Quantum Advanced Engineering Plastics |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM C177 |
Quantum Nylon 6/6 MoS2 Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Thermal Conductivity | >= 0.245 W/m-K | >= 1.70 BTU-in/hr-ft²-°F | ASTM C177 |
PolyOne Lubri-Tech™ PF-000/15T Polysulfone, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM C-177 |
Technetics Group Texolon™ 7865 PTFE
(Unverified Data**) Virgin PTFE for those applications not requiring the premium qualities of 8764 sheet.PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surfac.. |
|||
Thermal Conductivity | 0.245 - 0.259 W/m-K | 1.70 - 1.80 BTU-in/hr-ft²-°F | Average value: 0.252 W/m-K Grade Count:4 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM C177 |
Garlock 8764 PTFE Rubber Sheet Premium Grade Skived PTFE SheetInformation provided by Garlock Rubber Technologies |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | |
Saint-Gobain Rulon® XL Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM C177 |
ScanTube PTFE Tubing Information provided by ScanTube, Inc. |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM C177 |
Westlake Plastics Tempalux® 20% GF Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM C177 |
Ensinger Tecapeek® Polyetheretherketone (PEEK) Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance.Excellent flex.. |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM C177 |
Ensinger Tecapeek® Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM C177 |
Ensinger Tecapeek® XP-96 Compression Molded PEEK Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM C-177 |
Technetics Group Texolon™ 8764 PTFE
(Unverified Data**) A premium PTFE sheet manufactured from the highest quality PTFE.PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectri.. |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Nylatron® MC® 907 Natural Nylon, Monocast® FDA Compliant, Unfilled Type 6 (ASTM Product Data Sheet) |
|||
Thermal Conductivity | 0.245 W/m-K | 1.70 BTU-in/hr-ft²-°F | ASTM E1530-11 |
Quadrant EPP Quadrant Nylon 105 Black |