Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.232 W/m-K | 1.61 BTU-in/hr-ft²-°F | |
Sharadaa Ceramics REFINSUL 8S Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Thermal Conductivity | 0.232 W/m-K @Temperature 500 °C |
1.61 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Sharadaa Ceramics Sharada LTM 0.9 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Thermal Conductivity | <= 0.232 W/m-K @Temperature 500 °C |
<= 1.61 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Sharadaa Ceramics REFINSUL ZAP-015 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Thermal Conductivity | >= 0.233 W/m-K @Temperature 350 °C |
>= 1.61 BTU-in/hr-ft²-°F @Temperature 662 °F |
|
Chosun Refractories B-3 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | >= 0.233 W/m-K @Temperature 350 °C |
>= 1.61 BTU-in/hr-ft²-°F @Temperature 662 °F |
|
Chosun Refractories LW-24 Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | >= 0.233 W/m-K @Temperature 350 °C |
>= 1.61 BTU-in/hr-ft²-°F @Temperature 662 °F |
|
Chosun Refractories A-6 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |