Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | |
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NH9294 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NH9350 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
Quantum Modified PPO - Noryl® Information provided by Quantum Advanced Engineering Plastics |
|||
Thermal Conductivity | >= 0.231 W/m-K | >= 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
PolyOne Edgetek® AS-30GF/000 FRVO Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFlame RetardantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Thermal Conductivity | 0.230 - 0.500 W/m-K | 1.60 - 3.47 BTU-in/hr-ft²-°F | Average value: 0.261 W/m-K Grade Count:39 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL SE0 PPE+HIPS (Europe-Africa-Middle East) NORYL SE0 is an unfilled, flame retardant material with a Vicat B/120 of 130C according ISO 306. NORYL SE0 is V0 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL SE1 PPE+HIPS (Europe-Africa-Middle East) NORYL SE1 is an unfilled, flame retardant material with a Vicat B/120 of 140°C according ISO 306. NORYL SE1 is V1 at 1.47 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Conditioned Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Asia Pacific) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER PC+Polyester, UV Stabilized, Transparent |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Asia Pacific) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Noryl HF180 PPE+HIPS (Europe-Africa-Middle East) NORYL HF180 is an unfilled, flame retardant material with a Vicat B/120 of 100°C according ISO 306. NORYL HF180 is V1 at 2.0 mm according UL94 and halogenThis data was supplied by SABIC-IP for th.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Noryl HIN120P PPE+HIPS (Europe-Africa-Middle East) Noryl HIN120P is designed for selected one layer water-based paint systems. Noryl HIN120P has a Vicat B/120 of 120 °C and is targetedThis data was supplied by SABIC-IP for the Europe-Africa-Middl.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
ScanTube ETFE Tubing Information provided by ScanTube, Inc. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative) Carbon powder filled with high flexural strength and good thermal stability to 270°F. Thermoformable in 0.010" to 0.060" gauges; low outgassing.Information provided by Westlake Plastics. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 1200 G Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material wit.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 125 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 257 °F |
|
Dow SiLK™ I 550 Semiconductor Dielectric Resin SiLK™ I 550 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I 550 is compatible with.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 125 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 257 °F |
|
Dow SiLK™ I 620 Semiconductor Dielectric Resin SiLK™ I 620 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I 620 is compatible with.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 125 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 257 °F |
|
Dow SiLK™ I300 560 Semiconductor Dielectric Resin SiLK™ I300 560 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 560 is compatibl.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultradur B 4300 G2 10% Glass Filled PBT Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Thermal Conductivity | 0.230 - 0.418 W/m-K | 1.60 - 2.90 BTU-in/hr-ft²-°F | Average value: 0.255 W/m-K Grade Count:16 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | Melt |
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR30 HS is a heat stabilized 30% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Thermal Conductivity | 0.230 - 0.317 W/m-K | 1.60 - 2.20 BTU-in/hr-ft²-°F | Average value: 0.295 W/m-K Grade Count:4 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612-1 |
BASF Ultradur® B 4300 G2 FC 10% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |