Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 103 PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV stabilized for outdoor and lighting. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 123R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® FXE154 PC FDA compliant (color limited) PC. 2.5 MFR. Potable water/extrusion blowmoldable. ILLUMINATE special effects (fluorescent/edge glow colors). |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® HPS1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® LI1911R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C 177 |
SABIC Innovative Plastics Lexan® VR2020 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release.This data was supplied by SABIC-.. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 143 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. UV-stabilized. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® HP2NR PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | |
Permabond MM115 Anaerobic Threadlocker Permabond® MM115 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and maintenance... |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV6126 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM DH1004 PEI (Asia Pacific) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C 177 |
SABIC Innovative Plastics Ultem DH1004F PEI High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM HU1004 PEI High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. For medical devices and pharmaceutical applications. Healthcare management of change, biocomp.. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM HU1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Valox® 815UX PBT (Europe-Africa-Middle East) VALOX 815UX is a 15% glass reinforced PBT+PET blend with improved surface appearance and excellent UV performance. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM 9090 PEI (Europe-Africa-Middle East) Polyetherimide Blend with improved Ductility and Detergent resistance. Meets FAR 25.853 and OSU 55/55 heat release and provides low toxicity, smoke and flame evolution. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C177 |
Westlake Plastics Zelux® M Machine Grade Polycarbonate Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | |
Eastman Eastar DN004 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Eastman AP006 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | |
Hippe PMMA Components made of PMMA are brilliantly transparent. Outstanding aging stability and weathering resistance. Good surface hardness. Abrasion-resistant. Physiologically safe. High strength. Easi.. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | |
Dow SiLK™ I 620 Semiconductor Dielectric Resin SiLK™ I 620 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I 620 is compatible with.. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | |
Dow SiLK™ I300 380 Semiconductor Dielectric Resin SiLK™ I300 380 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 380 is compatibl.. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C177 |
Ensinger TECAFLON™ PVDF Polyvinylidene Fluoride (PVDF) - extruded products Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin which has good resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated solvent.. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | Silicone Property; ASTM E 1530 |
Arlon R37208T017 0.017" (0.432 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Liner Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionThis data represents typical values for the productio.. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | |
Permabond A1042 Anaerobic Threadlocker Permabond® A1042 is a rapid curing adhesive designed to lock and seal metal parts that subsequently may need to be dismantled for maintenance. The high vibration resistance makes Permabond A1042 pa.. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 953A PC Clear, tints and opaque colors, high viscosity, flame retardant with exceptional surface. UV-stabilized. |
|||
Thermal Conductivity | 0.190 - 0.303 W/m-K | 1.32 - 2.10 BTU-in/hr-ft²-°F | Average value: 0.281 W/m-K Grade Count:8 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | |
Permabond A131 Anaerobic Threadsealant Permabond® A131 is an anaerobic adhesive designed to seal threaded metal pipe connections carrying a wide variety of gases and liquids, including potable water. Suitable for use on both parallel an.. |