Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 1.289 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity >= 0.1861 W/m-K

@Temperature 350 °C
>= 1.289 BTU-in/hr-ft²-°F

@Temperature 662 °F
Chosun Refractories A-4 Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Thermal Conductivity >= 0.1861 W/m-K

@Temperature 350 °C
>= 1.289 BTU-in/hr-ft²-°F

@Temperature 662 °F
Chosun Refractories LW-23 Special Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).