Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.167 W/m-K | 1.16 BTU-in/hr-ft²-°F | Melt |
Covestro Apec® DP 1-9359/5 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Thermal Conductivity | 0.167 - 0.795 W/m-K | 1.16 - 5.52 BTU-in/hr-ft²-°F | Average value: 0.480 W/m-K Grade Count:20 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
Thermal Conductivity | 0.167 - 1.44 W/m-K | 1.16 - 10.0 BTU-in/hr-ft²-°F | Average value: 0.838 W/m-K Grade Count:12 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Thermal Conductivity | 0.167 - 0.300 W/m-K | 1.16 - 2.08 BTU-in/hr-ft²-°F | Average value: 0.292 W/m-K Grade Count:16 |
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum.. |
|||
Thermal Conductivity | 0.167 - 0.300 W/m-K | 1.16 - 2.08 BTU-in/hr-ft²-°F | ASTM C177 |
Zeus PTFE Tubing Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,.. |
|||
Thermal Conductivity | 0.167 W/m-K | 1.16 BTU-in/hr-ft²-°F | Melt |
Covestro Apec® 1800 Polycarbonate Basic gradesoftening temperature (VST/B 120)=185 °CPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.167 W/m-K | 1.16 BTU-in/hr-ft²-°F | Melt |
Covestro Apec® 1803 Polycarbonate UV-stabilizedsoftening temperature (VST/B 120)=184 °CPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.167 W/m-K | 1.16 BTU-in/hr-ft²-°F | Melt |
Covestro Apec® 1895 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=183 °CPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.167 W/m-K | 1.16 BTU-in/hr-ft²-°F | Melt |
Covestro Apec® 1897 Polycarbonate Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=182 °CPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.167 W/m-K | 1.16 BTU-in/hr-ft²-°F | Melt |
Covestro Apec® DP1-9354 Polycarbonate, Flame Retardant Grade Developmental productflame retardant: V-0/1,5mm (UL 94)V-0/3,0mm (UL 94)5VA/3mm (UL 94)softening temperature (VST/B 120)=185 °Conly opaque colors availablePreprocessingMax. Water content |
|||
Thermal Conductivity | 0.167 W/m-K | 1.16 BTU-in/hr-ft²-°F | Melt |
Covestro Apec® DP1-9354/1 Polycarbonate, Flame Retardant Grade Developmental productflame retardant: V-0/3,2mm (UL 94)V-2/1,5mm (UL 94),softening temperature (VST/B 120)=185 °Calso available in transparent colorsPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.167 W/m-K | 1.16 BTU-in/hr-ft²-°F | Melt |
Covestro Makroblend® KU 2-7912/5 Polycarbonate + PBT, Impact Grade Developmental productISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh flowhigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
Abatron AboCast/AboCure 50-24/8501-4 High Temperature Resistant Epoxy Clear amber, low viscosity, structural/dielectric epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components to.. |
|||
Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
Abatron AboCast/AboCure 8502-1 Epoxy AboCast/AboCure 8502-1 is a solventless clear Epoxy System, used as a casting, adhesive, and impregnating resin for transformers, capacitors, coils, and other electronic components requiring a low-v.. |
|||
Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
Abatron AboCast 8103-13 One-Component Epoxy AboCast 8103-13 is the low-viscosity one-component clear epoxy system with deep impregnation that offers high performance at relatively high temperatures. It is best for thin-wall casting. Suggested.. |
|||
Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
Abatron AboCast 8501-6 One-Component Epoxy AboCast 8501-6 is a clear, high-temperature one-component epoxy system for very high-temperature uses. It offers the highest heat resistance of the clear resins. Suggested Uses: Casting; Potting; E.. |
|||
Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
Abatron AboCast 8504-1 One-Component Epoxy AboCast 8504-1 is a clear, all-purpose one-component epoxy system, with an optimum balance of properties for most casting, adhesive, impregnation, and coating applications. |
|||
Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
Abatron AboCast 8504-5 One-Component Epoxy AboCast 8504-5 is a clear, plasticized one-component epoxy system with very high strength and impact. It provides exceptional physical properties and thermal shock resistance from sub-zero to modera.. |
|||
Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
Abatron AboCast/AboCure 8501-6/8501-4 High Temperature Resistant Epoxy 1-component system. Clear amber, low viscosity, structural/dielectric epoxy.Processing: Pot Life: 5-9 months. Cured 2 hours at 95°C + 15 hour post-cure at 230°C. Information provided by Abatron... |
|||
Thermal Conductivity | 0.167 W/m-K | 1.16 BTU-in/hr-ft²-°F | BS 874A |
Mitsui TPX® DX820 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Thermal Conductivity | 0.167 W/m-K | 1.16 BTU-in/hr-ft²-°F | BS 874A |
Mitsui TPX® MX002 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Thermal Conductivity | 0.167 W/m-K | 1.16 BTU-in/hr-ft²-°F | BS 874A |
Mitsui TPX® MX004 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Thermal Conductivity | 0.167 W/m-K | 1.16 BTU-in/hr-ft²-°F | BS 874A |
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Thermal Conductivity | 0.167 W/m-K | 1.16 BTU-in/hr-ft²-°F | BS 874A |
Mitsui TPX® RT18 XB Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
Abatron AboCast/AboCure 50-7/8501-4 High Temperature Resistant Epoxy Clear amber, high viscosity, structural/dielectric epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components t.. |