Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.152 W/m-K | 1.05 BTU-in/hr-ft²-°F | Melt |
Covestro Bayblend® KU 2-1446 Polycarbonate + ABS Blend
(discontinued **) Key Features:UnfilledPlatableSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bay.. |
|||
Thermal Conductivity | 0.151 W/m-K | 1.05 BTU-in/hr-ft²-°F | |
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Thermal Conductivity | 0.151 W/m-K | 1.05 BTU-in/hr-ft²-°F | Halar® 300 |
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Thermal Conductivity | 0.151 W/m-K | 1.05 BTU-in/hr-ft²-°F | Melt |
Covestro Bayblend® FR 3002 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradefor notebooks and thinwall applicationsVicat/B 120 temperature = 99 °CUL-listing 94 V-0 (1.2 mm)antimony- chlorine- and bromine-free flame retardantglow wire test (GWFI): 960.. |
|||
Thermal Conductivity | 0.152 W/m-K | 1.05 BTU-in/hr-ft²-°F | Melt |
Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeincreased heat resistanceVicat/B 120 temperature = 110 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (.. |
|||
Thermal Conductivity | 0.152 W/m-K | 1.05 BTU-in/hr-ft²-°F | Melt |
Covestro Bayblend® KU 1-1446* Polycarbonate + ABS Developmental productGrade with improved low-temperature impact strength and petrol resistance for automotive partsin version BBS904 suitable for extrusion/extrusion blow molding and electroplating .. |
|||
Thermal Conductivity | 0.151 W/m-K @Thickness 6.35 mm, Temperature 44.3 °C |
1.05 BTU-in/hr-ft²-°F @Thickness 0.250 in, Temperature 112 °F |
|
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.Information provided b.. |