Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.139 W/m-K @Temperature 600 °C |
0.965 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Sharadaa Ceramics Saber Block, Pyroblock Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Thermal Conductivity | 0.139 W/m-K @Temperature 500 °C |
0.965 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Sharadaa Ceramics Sharada LTM 0.4 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Thermal Conductivity | 0.139 W/m-K @Temperature 500 °C |
0.965 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Sharadaa Ceramics Sharada LTM 0.5 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Thermal Conductivity | 0.139 W/m-K | 0.965 BTU-in/hr-ft²-°F | Melt |
Covestro Desmopan® 481 Polyurethane injection molding gradefree from plasticizersgrease and oil-resistantlow compression sethigh elasticitygood heat resistanceEasy releaseApplicationRoller coatingSealsmembranesAutomotive engineeringPr.. |
|||
Thermal Conductivity | 0.139 W/m-K | 0.965 BTU-in/hr-ft²-°F | Melt |
Covestro Desmopan® DP 1485A Polyurethane Extrusion- and injection molding gradesuitable for extrusion blow moldingvery large processing windowhigh melt stabilityBeadsApplicationBellowsHosesnon-reinforcedProfilesInjection molded engineering.. |
|||
Thermal Conductivity | 0.139 W/m-K | 0.965 BTU-in/hr-ft²-°F | Melt |
Covestro Desmopan® DP 2590A Polyurethane Extrusion- and injection molding gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationBlown filmsPreprocessingMax. Water content.. |
|||
Thermal Conductivity | 0.139 W/m-K | 0.965 BTU-in/hr-ft²-°F | Melt |
Covestro Desmopan® DP 2786A Polyurethane Coating gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationTextile coatingPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.139 W/m-K | 0.965 BTU-in/hr-ft²-°F | Melt |
Covestro Desmopan® DP 2792A Polyurethane Coating gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationTextile coatingPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.139 W/m-K | 0.965 BTU-in/hr-ft²-°F | Melt |
Covestro Desmopan® DP 3491A Polyurethane Extrusion- and injection molding gradesuitable for extrusion blow moldinghigh mechanical strengthhigh melt stabilityApplicationBlow moldingProfilesInjection molded engineering partsPreprocessingMax... |
|||
Thermal Conductivity | 0.139 W/m-K | 0.965 BTU-in/hr-ft²-°F | Melt |
Covestro Desmopan® DP 3660DU Polyurethane Extrusion- and injection molding gradetransparent up to 6 mm wall thicknesshydrolysis-stabilisedwith special UV stabilizerswith release agentgood wear resistanceApplicationSports shoe solesHosesnon-.. |
|||
Thermal Conductivity | 0.139 W/m-K | 0.965 BTU-in/hr-ft²-°F | Melt |
Covestro Desmopan® DP 3690AU Polyurethane Extrusion- and injection molding gradehydrolysis-stabilisedwith special UV stabilizerswith release agenttransparent up to 6 mm wall thicknessgood wear resistanceApplicationSports shoe solesFilmsHose.. |
|||
Thermal Conductivity | 0.139 W/m-K | 0.965 BTU-in/hr-ft²-°F | Melt |
Covestro Desmopan® DP 3695AU Polyurethane Extrusion- and injection molding gradetransparent up to 6 mm wall thicknesshydrolysis-stabilisedwith special UV stabilizerswith release agentgood wear resistanceApplicationSports shoe solesHosesnon-.. |
|||
Thermal Conductivity | 0.139 W/m-K | 0.965 BTU-in/hr-ft²-°F | Melt |
Covestro Desmopan® DP 5080A Polyurethane injection molding gradeimproved microbial resistanceImproved hydrolysis resistanceApplicationSealsmembraneshard - soft systemsPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.139 W/m-K @Temperature 150 °C |
0.965 BTU-in/hr-ft²-°F @Temperature 302 °F |
|
DuPont™ Nomex® 410 Paper, 10 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |