Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.110 W/m-K | 0.763 BTU-in/hr-ft²-°F | ASTM C158 |
Rogers Corporation Bisco™ HT-820 Cellular Silicone Foam Firm grade silicone sponge. UL recognized for flame retardance.Applications: Gaskets where higher closure force is available or necessary, Cushions in heavier-load applicationsGasketing and sealing.. |
|||
Thermal Conductivity | 0.110 W/m-K | 0.763 BTU-in/hr-ft²-°F | DIN.52612 |
Omnia Plastica PVDF Kynar PVDF is a relatively new fluoropolymer. Like the other fluoropolymers, its best feature is its chemical resistance. The mechanical features of PVDF are notably higher than PTFE and it does not suffe.. |
|||
Thermal Conductivity | 0.110 - 0.150 W/m-K @Temperature 50.0 - 400 °C |
0.763 - 1.04 BTU-in/hr-ft²-°F @Temperature 122 - 752 °F |
|
Pyrotek Firefly 800 Roller & Furnace Cladding Material Firefly 800 is a beige asbestos-free material made from high-quality shot-free mineral wool and inert fillers. Rollers made of Firefly 800 are constructed to resist breakage in handling service. F.. |
|||
Thermal Conductivity | 0.110 - 0.150 W/m-K | 0.763 - 1.04 BTU-in/hr-ft²-°F | |
Pyrotek U-1 Compressible Board U-1 is a high-temperature millboard that is easily cut, punched and shaped. It works well as a roll-cladding material and as compressible gasketing. A unique characteristic of the asbestos-free bo.. |
|||
Thermal Conductivity | 0.110 - 0.300 W/m-K | 0.763 - 2.08 BTU-in/hr-ft²-°F | Average value: 0.182 W/m-K Grade Count:62 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Thermal Conductivity | 0.110 W/m-K | 0.763 BTU-in/hr-ft²-°F | |
Trelleborg Fillite® 160 Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Thermal Conductivity | 0.110 W/m-K | 0.763 BTU-in/hr-ft²-°F | |
Trelleborg Fillite® 160W Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Thermal Conductivity | 0.110 W/m-K | 0.763 BTU-in/hr-ft²-°F | |
Trelleborg Fillite® 52/7S (355) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Thermal Conductivity | 0.110 W/m-K | 0.763 BTU-in/hr-ft²-°F | |
Trelleborg Fillite® FG (300) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Thermal Conductivity | 0.110 W/m-K | 0.763 BTU-in/hr-ft²-°F | |
Trelleborg Fillite® SGHA (500HA) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Thermal Conductivity | 0.110 W/m-K | 0.763 BTU-in/hr-ft²-°F | |
Trelleborg Fillite® 106 Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Thermal Conductivity | 0.110 W/m-K | 0.763 BTU-in/hr-ft²-°F | |
Trelleborg Fillite® 300W Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Thermal Conductivity | 0.110 W/m-K | 0.763 BTU-in/hr-ft²-°F | |
Trelleborg Fillite® SG (500) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Thermal Conductivity | 0.110 W/m-K | 0.763 BTU-in/hr-ft²-°F | |
CMT Materials HYTAC® FLX Good Durability, Easily Machined & Polished Copolymer Syntactic HYTAC-FLX has been improved for optimum performance in transparent applications. The enhanced formulation is easy to polish and results in minimal to no scratches with transparent sheet materials. .. |
|||
Thermal Conductivity | 0.110 W/m-K | 0.763 BTU-in/hr-ft²-°F | |
Dow Corning XIAMETER® PMCPPMX-0210 Silicone Fluid 100CS Is chemically equivalent to DOW CORNING® 210H FLUID 100CS. This product is a heat stabilized polydimethlysiloxane, used for heat transfer.Information provided by Dow Corning |
|||
Thermal Conductivity | 0.110 W/m-K | 0.763 BTU-in/hr-ft²-°F | |
Trelleborg Fillite® PG (300LF) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Thermal Conductivity | 0.110 W/m-K | 0.763 BTU-in/hr-ft²-°F | |
Hippe PVDF Better mechanical strength compared to other fluorinated polymers. Tough and hard. High-grade electrical feature. Good weathering stability. Physiologically safe. Not as good as fluorinated pol.. |