Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0830 W/m-K @Temperature 150 °C |
0.576 BTU-in/hr-ft²-°F @Temperature 302 °F |
|
DuPont™ Nomex® E56 Paper, 10 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Thermal Conductivity | 0.0830 W/m-K @Temperature 150 °C |
0.576 BTU-in/hr-ft²-°F @Temperature 302 °F |
measured on 10 mil sample |
DuPont™ Nomex® E56 Paper, 12 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Thermal Conductivity | 0.0830 W/m-K @Temperature 150 °C |
0.576 BTU-in/hr-ft²-°F @Temperature 302 °F |
measured on 10 mil sample |
DuPont™ Nomex® E56 Paper, 15 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Thermal Conductivity | 0.0830 W/m-K @Temperature 150 °C |
0.576 BTU-in/hr-ft²-°F @Temperature 302 °F |
measured on 10 mil sample |
DuPont™ Nomex® E56 Paper, 20 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Thermal Conductivity | 0.0830 W/m-K @Temperature 150 °C |
0.576 BTU-in/hr-ft²-°F @Temperature 302 °F |
measured on 10 mil sample |
DuPont™ Nomex® E56 Paper, 5 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Thermal Conductivity | 0.0830 W/m-K @Temperature 150 °C |
0.576 BTU-in/hr-ft²-°F @Temperature 302 °F |
measured on 10 mil sample |
DuPont™ Nomex® E56 Paper, 7 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |