Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0349 W/m-K | 0.242 BTU-in/hr-ft²-°F | 25g/L; KS M 3808 |
LG Chemical B120 EPS, Non-Flame Retardant Feature: Expendable Polystyrene, Non-Flame RetardantApplication: Package, Fruit/Fish Box, Floats, Pad, Ice BoxCAS No. 9003-53-6 and 109-66-0Information provided by LG Chemical |
|||
Thermal Conductivity | 0.0349 W/m-K | 0.242 BTU-in/hr-ft²-°F | 30g/L; KS M 3808 |
LG Chemical B240 EPS, Non-Flame Retardant Feature: Expendable Polystyrene, Non-Flame RetardantApplication: Package, Fruit/Fish Box, Floats, Pad, Ice BoxCAS No. 9003-53-6 and 109-66-0Information provided by LG Chemical |
|||
Thermal Conductivity | 0.0349 W/m-K | 0.242 BTU-in/hr-ft²-°F | 25g/L; KS M 3808 |
LG Chemical R120 EPS, Flame Retardant Feature: Expendable Polystyrene, Flame RetardantApplication: Insulation Board, Sandwich Panel Civil Engineering & Construction MaterialsCAS No. 9003-53-6, 109-66-0, 3194-55-6 and 106-97-8Information.. |
|||
Thermal Conductivity | 0.0349 W/m-K | 0.242 BTU-in/hr-ft²-°F | 25g/L; KS M 3808 |
LG Chemical R160 EPS, Flame Retardant Feature: Expendable Polystyrene, Flame RetardantApplication: Insulation Board, Sandwich Panel Civil Engineering & Construction MaterialsCAS No. 9003-53-6, 109-66-0, 3194-55-6 and 106-97-8Information.. |
|||
Thermal Conductivity | 0.0349 W/m-K | 0.242 BTU-in/hr-ft²-°F | 30g/L; KS M 3808 |
LG Chemical R320 EPS, Flame Retardant Feature: Expendable Polystyrene, Flame RetardantApplication: Insulation Board, Sandwich Panel Civil Engineering & Construction MaterialsCAS No. 9003-53-6, 109-66-0, 3194-55-6 and 106-97-8Information.. |
|||
Thermal Conductivity | 0.0349 W/m-K | 0.242 BTU-in/hr-ft²-°F | 30g/L; KS M 3808 |
LG Chemical B320 EPS, Non-Flame Retardant Feature: Expendable Polystyrene, Non-Flame RetardantApplication: Package, Fruit/Fish Box, Floats, Pad, Ice BoxCAS No. 9003-53-6 and 109-66-0Information provided by LG Chemical |
|||
Thermal Conductivity | 0.0348 W/m-K | 0.242 BTU-in/hr-ft²-°F | 18 g/l; EN 12667 |
Jackon JACKOCELL® S314 Expanded Polystyrene Construction and Block Molding Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S314 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces ave.. |