Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0339 W/m-K | 0.235 BTU-in/hr-ft²-°F | |
NOVA Chemicals Dylite® F271TN Expandable Polystyrene Resin Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai.. |
|||
Thermal Conductivity | 0.0339 W/m-K | 0.235 BTU-in/hr-ft²-°F | |
NOVA Chemicals Dylite® F271TS Expandable Polystyrene Resin Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai.. |