Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 130.0 - 200.0 W/m-K | 902.2 - 1388 BTU-in/hr-ft²-°F | |
ALIMEX 2017A T451 Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress relieved by stretching a controlled amount and then naturally aged. |