Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 14.0 - 20.0 W/m-K | 97.2 - 139 BTU-in/hr-ft²-°F | |
Blasch Ceramics NITRON Nitride bonded SiC Features:Properties suit many severe operating conditionsGood wear and abrasionResists wetting by non-ferrous metalsHigh mechanical strengthExcellent Thermal shock resistance |
|||
Thermal Conductivity | 16.0 - 20.0 W/m-K | 111 - 139 BTU-in/hr-ft²-°F | in parallel (002) direction |
Momentive Performance Materials HOPG Graphite Monochromator Advanced Ceramics' graphite monochromators are highly oriented forms of high purity pyrolytic graphite which diffract x-rays and neutrons with greater efficiency than any other material. In x-r.. |