Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.330 - 1.15 W/m-K | 2.29 - 8.00 BTU-in/hr-ft²-°F | Average value: 0.553 W/m-K Grade Count:15 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |