Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.259 - 0.540 W/m-K | 1.80 - 3.75 BTU-in/hr-ft²-°F | Average value: 0.392 W/m-K Grade Count:6 |
Overview of materials for Polyamide-Imide, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Thermal Conductivity | 0.540 - 0.540 W/m-K @Temperature 100 - 100 °C |
3.75 - 3.75 BTU-in/hr-ft²-°F @Temperature 212 - 212 °F |
Average value: 0.540 W/m-K Grade Count:2 |
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi.. |