Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.300 - 0.401 W/m-K | 2.08 - 2.78 BTU-in/hr-ft²-°F | ASTM E1461-92 |
Park Electrochemical Nelco® N4000-2 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-2 is the most established material of Nelco’s product line. This multifunctional epoxy laminate and prepreg system has a long history of use and one of the broadest operating and .. |
|||
Thermal Conductivity | 0.300 - 0.401 W/m-K | 2.08 - 2.78 BTU-in/hr-ft²-°F | ASTM E1461-92 |
Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea.. |