Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.360 - 0.360 W/m-K | 2.50 - 2.50 BTU-in/hr-ft²-°F | Average value: 0.360 W/m-K Grade Count:4 |
Overview of materials for Polyamide-Imide, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Thermal Conductivity | 0.340 - 0.360 W/m-K | 2.36 - 2.50 BTU-in/hr-ft²-°F | Average value: 0.341 W/m-K Grade Count:15 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Thermal Conductivity | 0.340 - 0.360 W/m-K | 2.36 - 2.50 BTU-in/hr-ft²-°F | Average value: 0.344 W/m-K Grade Count:5 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Thermal Conductivity | 0.280 - 0.360 W/m-K | 1.94 - 2.50 BTU-in/hr-ft²-°F | |
Arlon 0.008" (0.2032 mm) Primerless Thermabond® Uncured Silicone (99990A008) 0.008 in., ±0.001 (0.2 mm, ±0.03) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in ±0.001(0.2 mm ± 0.03). T.. |
|||
Thermal Conductivity | 0.280 - 0.360 W/m-K | 1.94 - 2.50 BTU-in/hr-ft²-°F | |
Arlon 0.008" (0.2032 mm) Thermabond® Uncured Silicone (99510N008) 0.008 in., ±0.001 (0.2 mm, ±0.03) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in ±0.001(0.2 mm ± 0.03). T.. |
|||
Thermal Conductivity | 0.280 - 0.360 W/m-K | 1.94 - 2.50 BTU-in/hr-ft²-°F | |
Arlon 0.015" (0.381 mm) Primerless Thermabond® Uncured Silicone (99990A015) 0.015 in., ±0.001 (0.38 mm, ±0.038) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.015 in ±0.001(0.38 mm ± 0.038).. |
|||
Thermal Conductivity | 0.280 - 0.360 W/m-K | 1.94 - 2.50 BTU-in/hr-ft²-°F | |
Arlon 0.015" (0.381 mm) Thermabond® Uncured Silicone (99510N015) 0.015 in., ±0.001 (0.38 mm, ±0.038) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.015 in ±0.001(0.38 mm ± 0.038).. |
|||
Thermal Conductivity | 0.346 - 0.360 W/m-K | 2.40 - 2.50 BTU-in/hr-ft²-°F | Average value: 0.355 W/m-K Grade Count:3 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |
|||
Thermal Conductivity | 0.303 - 0.360 W/m-K | 2.10 - 2.50 BTU-in/hr-ft²-°F | Average value: 0.336 W/m-K Grade Count:9 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |