Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0240 - 0.0370 W/m-K @Temperature -80.0 - 50.0 °C |
0.167 - 0.257 BTU-in/hr-ft²-°F @Temperature -112 - 122 °F |
Average value: 0.0312 W/m-K Grade Count:5 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |
|||
Thermal Conductivity | 0.0240 - 0.0370 W/m-K @Temperature -80.0 - 50.0 °C |
0.167 - 0.257 BTU-in/hr-ft²-°F @Temperature -112 - 122 °F |
Average value: 0.0312 W/m-K Grade Count:1 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |
|||
Thermal Conductivity | 0.0240 - 0.0370 W/m-K @Thickness 50.0 - 50.0 mm |
0.167 - 0.257 BTU-in/hr-ft²-°F @Thickness 1.97 - 1.97 in |
Average value: 0.0312 W/m-K Grade Count:1 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |
|||
Thermal Conductivity | 0.0240 - 0.0370 W/m-K @Temperature -80.0 - 50.0 °C |
0.167 - 0.257 BTU-in/hr-ft²-°F @Temperature -112 - 122 °F |
Average value: 0.0312 W/m-K Grade Count:5 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Thermal Conductivity | 0.0240 - 0.0370 W/m-K @Temperature -80.0 - 50.0 °C |
0.167 - 0.257 BTU-in/hr-ft²-°F @Temperature -112 - 122 °F |
Average value: 0.0312 W/m-K Grade Count:1 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Thermal Conductivity | 0.0240 - 0.0370 W/m-K @Thickness 50.0 - 50.0 mm |
0.167 - 0.257 BTU-in/hr-ft²-°F @Thickness 1.97 - 1.97 in |
Average value: 0.0312 W/m-K Grade Count:1 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |