Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 60.0 W/m-K | 416 BTU-in/hr-ft²-°F | |
Poco Graphite ACF-10Q Industrial Grade Graphite POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr.. |
|||
Thermal Conductivity | 60.0 W/m-K | 416 BTU-in/hr-ft²-°F | |
Poco Graphite Glassmate® LT Graphite In very high wear situations, LT, with a hardness rating higher than GM material, will resist wear longer. |
|||
Thermal Conductivity | 60.0 W/m-K | 416 BTU-in/hr-ft²-°F | |
Poco Graphite SCF Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Thermal Conductivity | 60.0 - 90.0 W/m-K | 416 - 625 BTU-in/hr-ft²-°F | |
MMCC Al/Al2O3 3DP Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Thermal Conductivity | 60.0 W/m-K | 416 BTU-in/hr-ft²-°F | in "ab" direction |
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi.. |
|||
Thermal Conductivity | 60.0 - 120 W/m-K | 416 - 833 BTU-in/hr-ft²-°F | |
Momentive Performance Materials HCT-30 Titanium Diboride (TiB2) Powder A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u.. |
|||
Thermal Conductivity | 60.0 - 120 W/m-K | 416 - 833 BTU-in/hr-ft²-°F | |
Momentive Performance Materials HCT-30D Titanium Diboride (TiB2) Powder Grade HCT-30D is tailored for fabrication by the hot-pressing process. Its composition provides for ease and optimizes the mechanical properties of the component shapes.Titanium Diboride Powder .. |
|||
Thermal Conductivity | 60.0 - 120 W/m-K | 416 - 833 BTU-in/hr-ft²-°F | |
Momentive Performance Materials HCT-40 Titanium Diboride (TiB2) Powder A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u.. |
|||
Thermal Conductivity | 60.0 - 120 W/m-K | 416 - 833 BTU-in/hr-ft²-°F | |
Momentive Performance Materials HCT-F Titanium Diboride (TiB2) Powder Grade HCT-F powders are designed for use on applications requiring reduced particle size without sacrificing high purity.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced.. |
|||
Thermal Conductivity | 60.0 - 120 W/m-K | 416 - 833 BTU-in/hr-ft²-°F | |
Momentive Performance Materials HCT-S Titanium Diboride (TiB2) Powder Grade HCT-S powder can be cold-pressed and sintered into high density (98% of theoretical), near-net shapes.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced Ceramics usi.. |
|||
Thermal Conductivity | 60.0 - 80.0 W/m-K | 416 - 555 BTU-in/hr-ft²-°F | |
Goodfellow Tungsten Carbide/Cobalt Tungsten Carbide is a hard, brittle ceramic which, when combined with 6% to 10% Cobalt, forms a tough Cermet (Ceramic-Metal). This material was developed for use in cutting tools, having hard cerami.. |
|||
Thermal Conductivity | 60.0 W/m-K | 416 BTU-in/hr-ft²-°F | |
Cytec Thornel® T-605/50X 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.12000 filaments/strand.Thornel® products were sold by Amoco and are now owned by Cytec. |
|||
Thermal Conductivity | 60.0 W/m-K | 416 BTU-in/hr-ft²-°F | |
California Fine Wire Nickel Alloy 90 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Thermal Conductivity | 60.0 W/m-K | 416 BTU-in/hr-ft²-°F | in plane |
Carlisle 201HD Carbon-Carbon Composite Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t.. |
|||
Thermal Conductivity | 60.0 W/m-K | 416 BTU-in/hr-ft²-°F | |
Ceradyne CeraTrex™ 146-12E Silicon Carbide Features:corrosion resistancewear resistancetailored electrical propertiesApplications:semiconductor componentsInformation provided by Ceradyne Company |